The suitability of paper and printing and related processes (2)

Third, the printability of paper

In order to obtain prints with excellent print quality, paper and ink must be suitable materials. In other words, the requirements of the paper must be easy to print, in addition to the ink color is bright, strong coloring, but also must have good and proper permeability, volatility and the ability to conjunctiva. In addition, the rubber rollers, blankets, plates used in printing, and the conditions in the printing shop and the operation of the printing process must also be compatible with the need to print excellent works.

The printability of paper means that the paper can adapt to the requirements of the ink, printing plate, and printing conditions to ensure the smooth operation of the print job and obtain the necessary conditions for excellent prints. The printability of the paper is not a fixed property, but a performance that is compatible with different printing conditions and different print characteristics. (For reasons of space, we will briefly introduce some of the more important paper properties):

1. Brightness: In order to draw reader's attention to the strong printing contrast, you can use high-white paper, while low-white paper is more suitable for reading, books that are not easy to make your eyes tired. In Europe and the United States, books printed on low-white paper are very popular, and children's books in our country are moving closer to this aspect.

2, Color Colour: For different uses of paper, there are different requirements on the color, for industrial printing, except for special purposes, generally used are white paper.

3, gloss Gloss: Gloss changes will affect the color printing of color uniformity and print after print gloss. Uneven glossiness of the paper can cause prints to have different glosses, resulting in poor uniformity in reflection of the visual effects of the image. Too low gloss will result in prints with low gloss, poor color reproduction and dullness. The gloss is too high to affect the ink penetration, resulting in different drying speeds and back-printing problems (and back blemishes).

4, opacity Opacity: Grams weighing less than 105 grams of paper on the opacity is relatively high. If the opacity is too low, the image of the printed product may be easily printed. When the two sides are printed, the front and back images and characters may interfere with each other, affecting the visual effect. In particular, color printing may cause color cast, which may make color adjustment difficult.

5, ink absorption: ink absorption directly affects the quality of printed products, is one of the important properties of paper. For the same manufacturer, the absorbability of each batch of paper products must be uniform, and the same brand of paper products must also be consistent. Absorption of the ink is too small to cause printing dot enlargement, prone to print hair, back stains and long drying time; ink absorption is too high, will result in print penetration, ink pulverization, color change and deep image, clear Differences and other issues.

6. Surface strength: The higher the surface strength, the better. It is very important for offset printing. It includes the strength of IGT and the strength of wax extraction. If the surface strength is too low, the paint or fibers on the surface of the paper will be pulled up during printing. The surface of the print will cause spots and pits, foreign bodies on the surface of the blanket, and foreign matter in the ink fountain. In severe cases, the plate will wear. Due to the low surface strength caused by the waste and paper dust, cut paper powder, dust caused by the appearance of waste products have similarities, the difference in appearance is an important basis for the former can be found in the original point on the print, and the original point Concave, and the latter does not.

7. Moisture: Moisture content affects the change in size and curling of the paper. High moisture content also increases the runnability of uncoated paper. If the moisture content of coated paper is too high, blistering may occur on commercial web machines. At the same time, the moisture content of the paper must match that of the printing environment, otherwise curling of the single copper, the scalloping and the tight edge of the double copper offset paper may occur, and the overprint and the tight edges may cause overprinting. And printing folds and other issues. Excessive moisture in the paper can cause difficulties in feeding the paper, printing wrinkles, back-printing, curling, long drying time, and reduced stiffness; problems such as low water content can cause curling, difficulty in feeding paper, printing wrinkles, static electricity, and paper strength. Reduced and easily retractable issues.

8, smoothness smoothness roughness roughness: smoothness and roughness are the metrics of the micro-planarity of the paper surface, but the focus and the detection method is different. In gravure printing, the smoothness of the paper is required to be relatively high. If the smoothness is not enough, some dots cannot be transferred to the surface of the paper, resulting in dew point.

9, oil immersion foaming temperature: For commercial rotary coated paper, this physical property is very important. If the oil immersion foaming temperature does not reach a certain requirement, it cannot be used for rotary printing. Otherwise, blistering may easily occur during printing, resulting in the rejection of a large amount of printed matter.